Swine deep bedding ashes as a mineral additive for cement based mortar

The sustainability of intensive swine production demands alternative destinations for the generated residues. Ashes from swine rice husk-based deep bedding were tested as a mineral addition for cement mortars. The ashes were obtained at 400 to 600ºC, ground and sieved through a 325 mesh sieve (# 0.045 mm). The characterization of the ashes included the determination of the index of pozzolanic activity with lime. The ashes were also tested as partial substitutes of Portland cement. The mortars were prepared using a cement:sand proportion of 1:1.5, and with water/cement ratio of 0.4. Three percentages of mass substitution of the cement were tested: 10, 20 and 30%. Mortar performances were assessed at 7 and 28 days determining their compressive strength. The chosen condition for calcinations at the laboratory scale was related to the maximum temperature of 600ºC since the resulting ashes contained vitreous materials and presented satisfactory values for the pozzolanic index under analysis. The pozzolanic activity indicated promising results for ashes produced at 600ºC as a replacement of up to 30% in cement masses.

Saved in:
Bibliographic Details
Main Authors: Di Campos,Melissa Selaysim, Barbosa,Normando Perazzo, Savastano Jr.,Holmer
Format: Digital revista
Language:English
Published: Escola Superior de Agricultura "Luiz de Queiroz" 2008
Online Access:http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0103-90162008000200001
Tags: Add Tag
No Tags, Be the first to tag this record!